- South Korea / 2008
Ceramic fiber blanket
- ◾ Price: Negotiable
- ◾ MOQ: Negotiable
Ceramic fiber blanket
- ◾ Price: Negotiable
- ◾ MOQ: Negotiable
-
Required Quantity
-
Brand name-
-
Shipping / Lead TimeNegotiable / Negotiable
-
Keyword
-
Category
Specifications
| Size | - | Weight | - | Stock | - |
|---|---|---|---|---|---|
| Country of Origin | |||||
| Production method | Negotiable | ||||
Trade Terms
| Payment Terms | - | ||||
|---|---|---|---|---|---|
| Price(FOB) | Negotiable | MOQ | Negotiable | ||
| Transportation | - | ||||
| Lead time | Negotiable | Shipping time | Negotiable | ||
Company
-
Country / Year Established
-
Membership
- BIZ
Business typeManufacturer
-
Verified Certificate
-
12
-
12
Product Description
|
Items |
GBK-23(STD) |
GBK-23(DS) |
GBK-23(HDS) |
GBK-24(HDS) |
|
|
Needle Type |
Single |
Double-sided |
Double-sided |
Double-Sided |
|
|
Shot Content (%) |
≤ 15 |
≤ 15 |
≤ 15 |
≤ 15 |
|
|
Classification Temperature |
1260 ℃ |
1260 ℃ |
1260 ℃ |
1360 ℃ |
|
|
Working Temperature |
1100 ℃ |
1150 ℃ |
1150 ℃ |
1200 ℃ |
|
|
Color |
Pure White |
||||
|
Bulk Density (kg/m3) |
96-160 |
64-160 |
64-160 |
64-160 |
|
|
Shrinkage under Heating (%) |
1200OC x 24hrs ≤ -3.5 |
1200OC x 24hrs ≤ -3.5 |
1200OC x 24hrs ≤ -3.5 |
1250OC x 24hrs ≤ -3 |
|
|
Thermal Conductivity |
96kg/m3 128kg/m3 160kg/m3 |
||||
|
(W/m∙k) |
0.10(400℃) 0.09(400℃) 0.08(400℃) |
||||
|
|
0.17(600℃) 0.15(600℃) 0.11(600℃) |
||||
|
|
0.23(800℃) 0.20(800℃) 0.19(800℃) |
||||
|
Average Tensile Strength |
50 |
70 |
50 |
70 |
|
|
MPa (Density 128 kg/m3) |
|||||
|
Chemical Composition (%)
|
Al2O3 |
45 |
45 |
47 |
- |
|
Al2O3+SiO2 |
98 |
98 |
98.5 |
- |
|
|
AL2O3+SiO2+ ZrO2 |
- |
- |
- |
99 |
|
|
ZrO2 |
- |
- |
- |
>5 |
|
|
Fe2O3 |
0.3 |
0.3 |
0.3 |
0.2 |
|
|
Na2O3+K2O |
≤0.5 |
0.2 |
0.2 |
0.2 |
|
|
Products Item |
GBK-27(HPDS) |
GBK-29(HPDS) |
|
|
Needle Type |
Double-sided |
Double-sided |
|
|
Shot Content (%) |
≤ 10 |
≤ 10 |
|
|
Classification Temperature |
1500 |
1600 |
|
|
Color |
Green |
Pure White |
|
|
Bulk Density(kg/m3) |
64-160 |
96-160 |
|
|
Shrinkage under Heating (%) |
1400OC x 24hrs ≤ -2.5 |
1400OC x 24hrs ≤ -1.0 |
|
|
Thermal Conductivity (W/m∙k) |
128kg/m3 |
||
|
0.09(400℃) |
|||
|
0.12(600℃) |
|||
|
0.19(800℃) |
|||
|
Average Tensile Strength |
45 |
50 |
|
|
MPa (Density 128 kg/m3) |
|||
|
|
|
|
|
|
Chemical Composition (%) |
Al2O3 |
43 |
72 |
|
SiO2 |
54 |
28 |
|
|
Cr2O3 |
2.8 |
- |
|
|
Al2O3+SiO2+ Cr2O3 |
99 |
- |
|
|
Fe2O3 |
0.1 |
- |
|
|
Na2O3+K2O |
0.1 |
- |
|